Li(Ni0.5Co0.2Mn0.3)O2
Li(Ni0.5Co0.2Mn0.3)O2 Specifications Description Related Data D10 (μm) > 5.5 · X-ray diffraction pattern · Certificate of analysis · MSDS · Applications: Li-ion battery cathode material. · Warning: o Please keep the powder in vacuum box to avoid moisture. o Please bake the powder in a vacuum oven at 120 - 150 °C before making slurry and coating to ensure max. capacity D50 (μm) 10.5 – 14.5 D90 (μm) < 25.5 Dmax (μm) < 34.0 Appearance Dark brown powder, atmospheric stability Elements Proportions Ni:Co:Mn = 5:2:3 pH < 12 Specific Surface Area (m2/g) 0.25 - 0.42 Discharge Capacity (4.2-2.7V, mAh/g) 150-160 @0.2C vs. Li, Half Cell Coulomb Efficiency (3.0-4.3V, %) >85% Discharge Rate (%) 87.0 @3C vs. 0.2C Capacity Retention (RT, 3.0-4.3V, 1C, %) 93.8, 1C@51 cycles